OK you guys that do this all the time
can an 8' sheet of 6061T4 be bent 60 degrees with out cracking
this would be either .090 or .125 thick I'm in the design and
material selection stage?
what about if I have it intermittently cut leaving a series of
small tabs on the bend line the just tig the joint?
I know it can easily be done out of 16gauge steel, or even 304
same if use a 5000 series aluminum.
local shop would cut on laser and do the bend
why aluminum well weight savings and it won't rust.
end product will be painted
can an 8' sheet of 6061T4 be bent 60 degrees with out cracking
this would be either .090 or .125 thick I'm in the design and
material selection stage?
what about if I have it intermittently cut leaving a series of
small tabs on the bend line the just tig the joint?
I know it can easily be done out of 16gauge steel, or even 304
same if use a 5000 series aluminum.
local shop would cut on laser and do the bend
why aluminum well weight savings and it won't rust.
end product will be painted