mm
Aluminum
- Joined
- Mar 8, 2003
- Location
- NE Iowa, USA
I am having problems TIG welding 1 inch thin wall .065 stainless tubing. Pretty sure it is 316. The joints are all
coped pieces. We tacked the joints together. To try to control warpage, I am only welding about 1/4 of the
lenght, taking less than 45 seconds, then immediatly cooling with water. Even with this procedure, we are still
getting minor warping.
Please give me some suggestions.
TIA, mm
coped pieces. We tacked the joints together. To try to control warpage, I am only welding about 1/4 of the
lenght, taking less than 45 seconds, then immediatly cooling with water. Even with this procedure, we are still
getting minor warping.
Please give me some suggestions.
TIA, mm