Hey guys,
I have kind of a unique problem I hope someone can help with... I'm side milling a small 304 ss part and the process breaks through into an id feature at one point. The problem is that when it breaks through it is laying a very thin burr (like a piece of shim stock) down into the id area. That is what i'm trying to remedy. Is there a special type of end mill/process I should me using that would prevent this?
I have kind of a unique problem I hope someone can help with... I'm side milling a small 304 ss part and the process breaks through into an id feature at one point. The problem is that when it breaks through it is laying a very thin burr (like a piece of shim stock) down into the id area. That is what i'm trying to remedy. Is there a special type of end mill/process I should me using that would prevent this?