Marc von Amsberg
Plastic
- Joined
- Sep 20, 2011
- Location
- Charlotte, NC, USA
During quoting for a complicated (think 5-axis) part, I found protolabs additive manufactures and heat treats(!) this material. Here are Protolabs https://www.protolabs.com/media/1014635/stainlesssteel-17-4ph-material-spec-data-sheet-02.pdf and what I believe are the Stratasys spec sheets for the process (removed). I've been burned by other DMLS processes not working as planned, so I was wondering about others' experiences. This would be a high stress application, where the 170 ksi yield strength is critical.
It turns out Protolabs uses Concept laser, not Stratasys, so I removed that link.
It turns out Protolabs uses Concept laser, not Stratasys, so I removed that link.
Last edited: