Spruewell
Hot Rolled
- Joined
- Sep 8, 2015
- Location
- Northern California
Making some parts in 1” 2025 T-351 Aluminum. They are only .035 thick with an .065 thickness around the outside and tend to want to dish while parting. Tried grinding .065 thick thin-bits to reach, but had trouble with them breaking. Ran an indexable .125 parting tool, but it was eating up too much material.