countryboy1966
Hot Rolled
- Joined
- Jan 10, 2009
- Location
- Thompson, Ohio
I run parts had have high % material removal: lots of roughing minimal finishing. 6061-t6 al
I am going to set up with a separate roughing and finishing tool similar to the approach used on steel so I can control finishing dimensions longer.
Is this approach typical on aluminum as well? Checking to see so I don't buy all the extra tooling just for it not to work for an unforeseen issue.
Thanks!
I am going to set up with a separate roughing and finishing tool similar to the approach used on steel so I can control finishing dimensions longer.
Is this approach typical on aluminum as well? Checking to see so I don't buy all the extra tooling just for it not to work for an unforeseen issue.
Thanks!