I think I made a big mistake by ordering an aluminum plate that was hard anodized. I was surprised that it wasn't even deburred before anodizing, so now I'm stuck with deburring it myself. I forgot how hard the stuff is, so I tried using a file, which is now smooth. I also need to drill some holes. Any suggestions on what to use to deburr the edges? Any helpful techniques for drilling? Next time I'll have it anodized after machining (head slap).