david n
Diamond
- Joined
- Apr 13, 2007
- Location
- Pillager, MN
So is 17-4 offered in H900 condition? All I'm coming up with in my area is annealed or H1150. Parts need to be H900 when complete. So instead of machining annealed and sending off to HT, I'd like to just start out with H900. IIRC it should be OK to machine hardened. Drillin, boring, OD groovin, OD threadin, and part off....................May even have annealed bars sent off for HT if I can't find what I want..............or am I looney?